What is the plywood veneer production line
The plywood veneer production line is a series of processes for the production of glued veneer. First, ordinary cheap logs are cut to length and softened. This is the first step in the plywood veneer production line. After the wood has completely softened, it is sawn and cut. When cutting, cut the saw according to the requirements of straight grain or mountain pattern.
Then, the wood is sliced with a planer knife according to different thickness requirements and stacked manually, and then the rough edges of the slices are cut off with a cutter to form slices of different widths. Next, in the plywood veneer production line, the thin wood is clipped in a stripping pool with special tools until the color of the original wood is completely removed. The chemical solution on the thin wood is then thoroughly filtered out with clean water, and then placed in a dyeing tank for heating and dyeing. At this time, the most important thing is to master the proportion and temperature of the pigment. Usually, the color matching is carried out by the computer according to the target color, the color ratio and mass ratio of each clock are analyzed, and then the material is accurately weighed in proportion.
After that, the next step of the plywood veneer production line will be carried out. The dyed veneer needs to be dried by 70% before it is used for veneer. For plywood substrate, it is also necessary to enter the plywood production line at this time.
Defects affecting the smoothness of the finished product must be dealt with before grinding. Thereafter, according to the luster of the thin wood, the corresponding coloring covering agent is selected for coloring and drying, so that the color of the substrate and the thin wood is unified and kept dry. Then, in the plywood veneer production line, glue needs to be prepared. Manually paste the plywood onto the substrate to form a plywood blank board. Board Blank boards need to be collected and stacked manually. Enter the cold press for cold pressing to speed up initial bonding. Usually, it can be sent out after 1-2 hours to cut off the fine wood filament. After that, it is examined and considered to have been cured and polished.